Acid-resistant and heat-resistant ceramic tubes, acid-resistant bricks
Keywords:
Product Description
- 产品描述
-
Acid-resistant ceramic tube Made from high-quality local kaolin, refractory clay, porcelain stone, and other raw materials through strict batching, ball milling, vacuum kneading, and extrusion processes.
The back of the acid-resistant ceramic tube can also be equipped with dovetail grooves, facilitating firm bonding with acid-resistant mortar during construction, preventing detachment, ensuring project quality, and extending service life.
Advantages of acid-resistant and heat-resistant ceramic tubes:
1. Acid-resistant and heat-resistant ceramic tubes feature high acid resistance and low water absorption.
2. Acid-resistant and heat-resistant ceramic tubes are not easily oxidized or contaminated by media at room temperature.
3. Acid-resistant and heat-resistant ceramic tubes have excellent corrosion resistance to acids such as wet chlorine, brine, hydrochloric acid, sulfuric acid, and nitric acid.
4. Acid-resistant and heat-resistant ceramic tubes have excellent corrosion resistance to alkalis of any concentration at room temperature.
Acid-resistant and heat-resistant brick plates Used as linings for various tanks, towers, vats, and mixing pools in non-ferrous metal smelting, chemical, fertilizer, and power industries, these are special materials resistant to high temperature, cold, and strong acid corrosion.
Acid-resistant and heat-resistant ceramic tile tubes Technical parameters
Item Content
High-purity low-silicon corundum brick
Corundum bricks and corundum furnace tube cores
Special corundum products
AL ₂ O ₃ %≥
98.5
80–98
90
SiO ₂ %≤
0.5
Fe ₂ O ₃ %≤
0.2
0.5
0.5
Apparent porosity %≤
20
24–20
20
Bulk density g/cm³≥
3.1
2.6–3.1
2.85
Room temperature compressive strength MPa≥
50
30–50
50
Load softening point ℃≥
1700
1500–1700
1600
Reburning linear change rate %≤
1600℃ 3h 0.2
1500–1600℃ 3h 0.5
1600℃ 3h 0.5
Thermal expansion coefficient ×10⁻⁶/℃
1300℃ 8.6
1300℃ 8.6
1300℃ 8.6
Thermal conductivity W/(m·K)≤
2.0
2.0
2.0
Thermal stability 1100℃ water cooling cycles≥
12
8
12
Main crystal phase
a-AL ₂ O,
a-AL ₂ O ₃
a-AL ₂ O ₃
Acid-resistant brick Technical parameters
Item Content
Bulk density
Open porosity
Water absorption
Thermal stability
Elasticity degree
Tensile and compressive strength
Thermal conductivity
Thermal expansion coefficient
Acid resistance
Unit
g/cm2
%
%
950–20℃
MPa
MPa
w/mk
1/℃
%
Index
2.21–2.24
93–10.5
4.2–47
No cracking after 3 cycles
2138
123
1.175
3.8×10⁻⁶
99.8